Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar Flex® 2850-02 - PVDF - ARKEMA

Material Data Center offers the following functions for Kynar Flex® 2850-02:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kynar Flex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Kynar Flex® resins are fluorinated thermoplastic copolymers. 

Kynar Flex® 2850-02 has been specifically designed for use in wire and cable constructions which require an Underwriters Laboratories temperature of 150ºC and a Limiting Oxygen Index (LOI) of at least 75.

Kynar Flex® 2850-02 is easily processed and has excellent physical, mechanical, thermal and flame resistant characteristics.  Kynar Flex® 2850-02 meets the smoke and flame requirements of UL 910 and ASTM E84 (the Modified Steiner Tunnel Test).  This copolymer is commonly used for pipe, wire jacketing, conduits, and in injection molded parts.

ADDITIONAL CHARACTERISTICS
• Excellent thermal stability
• Excellent abrasion resistance
• Impervious to UV degradation
• Self extinguishing material
• Extremely low smoke emission characteristics
• 0/0 rating in ASTM E-84/UL 723


Main applications:
  • injection molded applications requiring the high chemical and temperature resistance properties of Kynar 2850-00 resin
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 15 cm³/10min ISO 1133
温度 232 °C -
载荷 3.8 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 1300 MPa ISO 527
屈服应力 40 MPa ISO 527
屈服伸长率 10 % ISO 527
名义断裂伸长率 >50 % ISO 527
简支梁缺口冲击强度, +23°C 8 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 157 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min -40 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 46 °C ISO 75-1/-2
1.5mm名义厚度时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
燃烧性-氧指数 43 % ISO 4589-1/-2
典型数据
加工方法
注塑, 电线挤出
特征
共聚物
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.